断裂伸长率 | ASTM D638/ISO 527 | 2.5-4.5 | % | |
拉伸强度 | ASTM D638/ISO 527 | 1000-1400 | kg/cm²(MPa)[Lb/in²] | |
洛氏硬度 | ASTM D785 | 94 | ||
弯曲模量 | ASTM D790/ISO 178 | ≥70000 | kg/cm²(MPa)[Lb/in²] |
燃烧性(率) | UL94 | V-0 |
耐电弧性 | ASTM D495/IEC 60112 | 100 |
断裂伸长率 | ASTM D638/ISO 527 | 2.5-4.5 | % | |
拉伸强度 | ASTM D638/ISO 527 | 1000-1400 | kg/cm²(MPa)[Lb/in²] | |
洛氏硬度 | ASTM D785 | 94 | ||
弯曲模量 | ASTM D790/ISO 178 | ≥70000 | kg/cm²(MPa)[Lb/in²] |
燃烧性(率) | UL94 | V-0 |
耐电弧性 | ASTM D495/IEC 60112 | 100 |